Sean: Yes, you can just fine sand the hot coat. Usually an acrylic sealant such as “Future” floor wax is applied after the fine sanding (see archives under Herb Spitzer). Yes, a gloss coat would provide a stronger sealant.You could just fine sand it if you don’t want a glossy finish. Personally, I would go for the gloss if a little weight is not a big issue. Take care and have fun. Patrick
Cobalt is a promoter used in resin to react with the MEKP. Mix the two together directly and you will have an explosion. YOU SHOULD NOT USE THIS IF YOU DO NOT NO WHAT YOUR DOING!!! Sluggo
nor will they pour it into smaller containers that I might afford. Per Jim F, because it’s too dangerous. He told me it could be, and had been, used to make bombs. I snickered and said there were better ways to make bombs than with cobalt…
hello guys, what should i put to my resin (reichold) to make it look blue like the silmar to glass my boards?
thanks
two drops of blue tint...