Glassing a longboard. Got enough 6oz for 2 layers only but plenty of 4oz. Should I do 2x6oz deck and 1x4oz bottom or 2x4oz bottom ? Thanks
I’m not a pro LB builder.
But my inclination would be to go 4x6 deck, plus 4-oz deck pad.
And 4x6 on the bottom.
See Gene’s post regarding symmetrical glassing schedule at this link,
1 Like
Yes I wondered about that too, just was a little worried bout wetting out 3 layers !!! Thanks for the link too
Laminate the 3rd layer separately.