How many CC’s of catalyst should I use per quart of resin? And another question: is it Ok for the laps to overlap each other? Does that cause any kind of thickness differences around the board? Thanks
what temp. are you working in?
Here a good reference. http://www.fiberglasssupply.com/pdf/miscellaneous/MEKPChart.pdf You might test a few small batches to determine setup time. On your first few boards there is no such thing as enough time! http://www.viser.net/~anthwind/
About 70*F