Hey guys,
Wondering if anyone vacuumes both sides of the board at the same time? this would realy speed up my glassing. If so any tricks or things i should know?
Hey guys,
Wondering if anyone vacuumes both sides of the board at the same time? this would realy speed up my glassing. If so any tricks or things i should know?
There’s plenty info in the archives on one-step lamination…just put it in a bag if you have the motivation…it won’t be any faster or cheaper with all the bag time and materials, but you should be able to reduce a tiny amount of resin volume if that’s what you are trying to do.
contrary to Wildy’s comment …
up side , it will halve your bagging time…
down side , if you dont get it right first time , youve pretty much stuffed your board or will have a way harder time recovering it…
if your talking high density core , with thin laminate skins , its a no brainer …
1lb or less , and you have challenges to over come and will need way more infrastructure to do it effectively and probably not worth the effort and cost in a back yard set up…
production faclity , for sure , its how it should be done …
regards